Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® T KR 4357 G6 - PA6T/6-I-GF30 - BASF

Material Data Center offers the following functions for Ultramid® T KR 4357 G6:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid T datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Glass fibre reinforced, impact modified, partially aromatic polyamide for injection molding. High toughness, stiffness and strength, low water absorption, high melting point (295°C).
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.4 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.0 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 9300 / 9000 MPa ISO 527
Contrainte à la rupture 165 / - MPa ISO 527
Déformation à la rupture 3.5 / - % ISO 527
Module de fluage en traction, 1000h * / 6500 MPa ISO 899-1
Résistance au choc Charpy, +23°C 95 / - kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 17 / - kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 295 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 105 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 240 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 285 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 22.5 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 65 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Yellow Card disponible oui / * - -
Aptitude à l'allumage 24 / * % ISO 4589-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 4.3 / 4.5 - IEC 62631-2-1
Facteur de pertes, 1MHz 300 / 400 E-4 IEC 62631-2-1
Résistivité transversale 1E13 / 1E12 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E13 Ohm IEC 62631-3-2
Indice de résistance au cheminement - / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 4.5 / * % Sim. to ISO 62
Absorption d'humidité 0.8 / * % Sim. to ISO 62
Masse volumique 1370 / - kg/m³ ISO 1183
Propriétés spécifiques à la matièresec / condUnitéNorme du test
ISO Data
Indice de viscosité 130 / * cm³/g ISO 307, 1157, 1628
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 110 °C -
Pré-séchage - temps 8 h -
L'humidité de traitement ≤0.15 % -
Température de la matière fondue 310 - 330 °C -
Température du moule 80 - 120 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Ultramid® T KR 4357 G6, PA6T/6-I-GF30, BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultramid® T KR 4357 G6, PA6T/6-I-GF30, BASF
Contrainte / Déformation , Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Contrainte / Déformation , Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Module sécant / Déformation , Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Module sécant / Déformation , Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Contrainte / Déformation (isochrone) 23°C, Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Module de fluage / Temps 23°C, Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Courbe de fluage 23°C, Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Contrainte / Déformation (isochrone) 90°C, Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Module de fluage / Temps 90°C, Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Courbe de fluage 90°C, Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Contrainte / Déformation (isochrone) 120°C, Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Module de fluage / Temps 120°C, Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Courbe de fluage 120°C, Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Volume spécifique (pvT) , Ultramid® T KR 4357 G6, PA6T/6-I-GF30, BASF
Module de traction / Température , Ultramid® T KR 4357 G6 (sec), PA6T/6-I-GF30, BASF
Module de traction / Température , Ultramid® T KR 4357 G6 (cond.), PA6T/6-I-GF30, BASF
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 110 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 310 - 330 °C
injection molding, Melt temperature, recommended: 320 °C
injection molding, Mold temperature, range: 80 - 120 °C
injection molding, Mold temperature, recommended: 100 °C
injection molding, Dwell time, thermoplastics: 5 min
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.